![]() Method for manufacturing aluminum oxide film for use in a semiconductor device
专利摘要:
A method for manufacturing an aluminum oxide film for use in a semiconductor device which includes the following steps: preparing a semiconductor substrate and setting the semiconductor substrate in a reaction chamber; supplying modified trimethyl aluminum (MTMA) as an aluminum source material into the reaction chamber so that it could be absorbed on the semiconductor substrate; discharging unreacted MTMA or by-product through a first pump by permitting nitrogen gas to flow into the reaction chamber and purging the chamber for vacuum status; supplying an oxygen source into the reaction chamber so that it could be absorbed on the semiconductor substrate; and discharging an unreacted oxygen source or by-product through a second pump by permitting nitrogen gas to flow into the reaction chamber and purging the chamber for vacuum status. 公开号:US20010006835A1 申请号:US09/739,444 申请日:2000-12-19 公开日:2001-07-05 发明作者:Min-Soo Kim;Kyong-Min Kim;Chan Lim;Heung-Sik Kwak;Chung-Tae Kim 申请人:Hyundai Electronics Industries Co Ltd; IPC主号:H01L21-3162
专利说明:
[0001] The present invention relates to a method for manufacturing a semiconductor device; and, more particularly, to a method for manufacturing an aluminum oxide in the semiconductor device by using a modified trimethyl aluminum (MTMA) as aluminum source material. [0001] DESCRIPTION OF THE PRIOR ART [0002] As is well known, a semiconductor memory device has a higher degree of integration because of downsizing through micronization. However, there is still a demand for downsizing the area of the memory cell, under increased transistor and circuit speeds and improved reliability. Demands for increased density, performance and reliability require the formation of device features with high precision and miniaturization. To meet the demands, it is necessary to increase the capacitance of a capacitor and improve the gate dielectric film which is applied to the DRAM and logic devices. In an attempt to solve a requirement, various researches have been made to employ the high dielectric materials for a capacitor thin film and a gate dielectric film. [0002] [0003] Aluminum oxide (Al[0003] 2O3) is typically used among high dielectric materials for the capacitor thin film and the gate dielectric thin film because aluminum oxide has good oxidation resistance and thermal stability. Furthermore, it can be used as a hydrogen barrier to prevent hydrogen diffusion. [0004] Aluminum oxide can be formed by using a method such as an atomic layer deposition (ALD). The manufacturing steps are as follows: setting a wafer in a chamber; heating up the wafer to 200° C. to 450° C.; supplying aluminum source material into the chamber; permitting nitrogen gas (N[0004] 2) to flow into the chamber and purging the chamber for vacuum status in order to sweep off unreacted aluminum source material or by-product; supplying an oxygen source material into the chamber; and permitting nitrogen gas to flow into the chamber and purging the chamber again for vacuum status in order to sweep off unreacted oxygen source material or by-product. The intended thickness of the aluminum oxide film is obtained by repeating the steps listed above. [0005] In a conventional method for manufacturing the aluminum oxide film in the semiconductor device, trimethyl aluminum (TMA) and water (H[0005] 2O) are mainly employed as the aluminum source material and the oxygen source material, respectively. TMA has a high vapor pressure and the difference between the boiling and melting points are very small. Therefore, it has drawbacks of strong explosiveness and inflammability when it is exposed in the atmosphere. Thus, TMA is not appropriate as the aluminum source material for manufacturing the aluminum oxide film for various uses in the semiconductor device. SUMMARY OF THE INVENTION [0006] It is, therefore, an object of the present invention to provide a method for manufacturing an aluminum oxide film by using modified trimethyl aluminum (MTMA) as an aluminum source material because it is stable in the atmosphere. [0006] [0007] In accordance with one aspect of the present invention, a method for manufacturing an aluminum oxide film for use in a semiconductor device is provided. The method comprises the following steps: a) preparing a semiconductor substrate and setting the semiconductor substrate in a reaction chamber; b) supplying modified trimethyl aluminum (MTMA) as an aluminum source into the reaction chamber so that it can be absorbed on the semiconductor substrate; c) discharging unreacted MTMA or by-product through a first discharge pump by flowing nitrogen gas into the reaction chamber and purging the chamber for vacuum status; d) supplying an oxygen source into the reaction chamber so that it can be absorbed on the semiconductor substrate; and e) discharging the unreacted oxygen source or by-product through a second discharge pump by permitting nitrogen gas to flow into the reaction chamber and purging the chamber for vacuum status. [0007] [0008] In accordance with another aspect of the present invention, a method for manufacturing a semiconductor device is provided. The method comprises the following steps of: a) preparing an active matrix with isolation regions, a substrate, gate line, gate oxide and a first insulating layer; b) forming a buffer layer and a first conductive layer on the active matrix; c) forming a dielectric layer of aluminum oxide (Al[0008] 2O3) on the first conductive layer by using an ALD method, MTMA being used as aluminum source; d) material obtaining a capacitor structure by forming a second conductive layer on the dielectric layer and patterning the second conductive layer, the dielectric layer, the first conductive layer and the buffer layer; e) forming a hydrogen barrier layer on the capacitor structure; f) forming a bit line and a local interconnection after depositing a second insulating layer; and g) forming a passivation layer on the bit line, the local interconnection and second insulating layers. BRIEF DESCRIPTION OF THE DRAWINGS [0009] The present invention will become more fully understood from the detailed description given herein below and the accompanying drawings which are given by way of illustration only, and thus are not limitative of the present invention, and wherein: [0009] [0010] FIGS. 1A to [0010] 1E are cross sectional views setting forth a method for manufacturing a semiconductor device incorporating aluminum oxide film in accordance with the preferred embodiment of the present invention; and [0011] FIG. 2 is an apparatus for depositing an aluminum oxide film by an atomic layer deposition (ALD) technique. [0011] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS [0012] Referring to FIGS. 1A to [0012] 1E, there are cross sectional views provided setting forth a method for manufacturing a semiconductor device incorporating therein an aluminum oxide in accordance with a preferred embodiment of the present invention. [0013] The process for manufacturing the semiconductor device begins with the preparation of an active matrix [0013] 110 including the following semiconductor substrate 102, an isolation region 104, diffusion regions 106A and 106B, a gate oxide 112, a gate line 113, a spacer 114 and a first insulating layer 116. One of the diffusion regions 106 serves as a source and the other diffusion region 106 serves as a drain. [0014] Thereafter in FIG. 1A, a buffer layer [0014] 118, a first conductive layer 120, a dielectric layer 122 and a second conductive layer 124 are formed on top of the active matrix 118. The dielectric layer 122 in the preferred embodiment is made of aluminum oxide (Al2O3) with a thickness ranging from 30Å to 100Å which is obtained by using a method such as an ALD, wherein the deposition pressure is approximately 50 to 300 mTorr. The buffer layer 118 is formed to improve adhesion between the first insulating layer 116 and the first conductive layer 120. [0015] The method for depositing the aluminum oxide of the dielectric layer [0015] 122 is illustrated in more detail below. [0016] In FIG. 2, a schematic diagram is shown setting forth an apparatus [0016] 200 for depositing aluminum oxide by an ALD method. Initially, the wafer is heated up to 200° C. to 450° C. and then aluminum source material, such as modified trimethyl aluminum (MTMA) 212, is supplied into the chamber 220 so that it could be absorbed on the wafer through a first flow controller (F/C) 214. Then the unreacted MTMA or by-product is discharged through a pump by permitting nitrogen gas to flow into the chamber 220 and the chamber is purged for a vacuum status. In the next step, the oxygen source material 216, such as H2O, O2, N2O or O3, is supplied into the chamber 220 so that it could be absorbed on the wafer through a second flow controller (F/C) 218. Then the unreacted oxygen source material or by-product is discharged through another pump. Each step is carried out for 0.1˜3 seconds. [0017] By repeating the steps listed above, it is possible to obtain the intended thickness of the aluminum oxide film. In addition, in order to use MTMA as the aluminum source material, it is required to equip a jacket heater for keeping the temperature of the MTMA vessel up to 50° C. to 100° C., and a line heater for keeping the temperature of a supply-line up to 70° C. to 180° C. It is important that the temperature of the chamber should be kept 200° C. to 450° C., and the pressure should be kept 50 mTorr to 300 mTorr so that the aluminum oxide can be effectively deposited on the wafer. [0017] [0018] After depositing the aluminum oxide, an oxygen treatment, such as plasma N[0018] 2O or ultra violet ozone (UV/O3), is carried out for removing carbon particles produced from the reaction. Then the annealing process is performed to densify the aluminum oxide film. [0019] Referring back to FIG. 1A, after layers [0019] 118, 120, 122, 124 are formed on the first insulating layer 116, the second conductive layer 124 is patterned into a first predetermined configuration to form a top electrode 124A. Then the dielectric layer 122, the first metal layer 120 and the buffer layer 118 are patterned into a second predetermined configuration, thereby forming a capacitor structure 150 having a buffer 118A, a bottom electrode 120A, a capacitor thin film 122A and a top electrode 124A, as shown in FIG. 1B. The bottom electrode 120A has a different size from the top electrode 124A so that a plate line could form (not shown) during the following processes. [0020] In the next step as shown in FIG. 1C, a hydrogen barrier layer [0020] 140 of an aluminum oxide is formed on the capacitor structure 150 and portions of the first insulating layer 116 with a thickness ranging preferably from 60 to 200Å, for preventing the capacitor structure 150 from experiencing hydrogen penetration during a post manufacturing process, such as a passivation process. Since, the method of forming the aluminum oxide layer by the ALD technique is same as that of the capacitor thin film 122A, the detailed description is abbreviated here. [0021] A second insulating layer [0021] 130 is formed on the capacitor structure 150 and the first insulating layer 116. Then the resulting structure is patterned into a third predetermined configuration, thereby obtaining openings 132, 134, 136 as shown in FIG. 1D. In a subsequent step, a third conductive layer is formed on the entire surface including the interiors of the openings 132, 134, 136 and patterned so that a bit line 144B and a local interconnection 144A are obtained. A passivation layer 152 is then formed on the entire surface by using a CVD or PVD method as shown in FIG. 1E. [0022] In the embodiment of the present invention, the gate oxide film [0022] 112 can be made of aluminum oxide by using the MTMA as the aluminum source material. [0023] Additionally, the aluminum oxide that is formed can be applied to an oxide or a polysilicon etch stop, but it is not limited to that. [0023] [0024] In comparison with the prior art which uses trimethyl aluminum (TMA) as the aluminum source material, the present invention provides a more stabilized fabrication method and a decrease in cost, as represented in table 1. [0024] TABLE 2 TMA MTMA Phase Liquid Liquid Boiling point 20° C./vacuum 50° C./vacuum Melting point 15.4 30 Vapor pressure 100 Torr (at 100° C.) 4 Torr (at 100° C.) Molecular weight 72 157 Safety inflammability/ stable (at ATM) explosiveness (at ATM) Cost expensive cheap [0025] Additionally the MTMA is not affected by a temperature change since a difference between the boiling point and the melting point of the MTMA is larger than that of the TMA and, the vapor pressure of the MTMA is lower than that of the TMA so that the manufacturing process is controlled easier than the prior art of the TMA being used as the aluminum source material. Although the MTMA is exposed on the atmosphere, it is still more stable than the TMA. [0025] [0026] The aluminum oxide can be formed through a stabilized manufacturing process if MTMA is used as the aluminum source in accordance with the present invention. [0026] [0027] Although the preferred embodiments of the invention have been disclosed for illustrative purposes, those skilled in the art will appreciate that various modifications, additions and substitutions are possible, without departing from the scope and spirit of the invention as disclosed in the accompanying claim. [0027]
权利要求:
Claims (16) [1" id="US-20010006835-A1-CLM-00001] 1. A method for manufacturing an aluminum oxide film for use in a semiconductor device, comprising the steps of: (a) preparing a semiconductor substrate and setting the semiconductor substrate in a reaction chamber; (b) supplying modified trimethyl aluminum (MTMA) as an aluminum source into the reaction chamber so that it can be absorbed on the semiconductor substrate; (c) discharging unreacted MTMA or by-product through a first discharge pump by permitting nitrogen gas to flow into the reaction chamber and purging the chamber for vacuum status; (d) supplying an oxygen source into the reaction chamber for being absorbed on the semiconductor substrate; and (e) discharging unreacted oxygen source or by-product through a second discharge pump by permitting nitrogen gas to flow into the reaction chamber and purging the chamber for vacuum status. [2" id="US-20010006835-A1-CLM-00002] 2. The method of claim 1 , wherein the steps (b) to (e) are repeated by using an atomic layer deposition (ALD) method until the aluminum oxide is formed on the semiconductor substrate to a predetermined thickness. [3" id="US-20010006835-A1-CLM-00003] 3. The method of claim 1 , wherein a temperature of the semiconductor substrate is in the range of 200° C. to 450° C. [4" id="US-20010006835-A1-CLM-00004] 4. The method of claim 1 , wherein the step (b) is carried out for 0.1 to 3 seconds. [5" id="US-20010006835-A1-CLM-00005] 5. The method of claim 1 , wherein the temperature of a vessel for storing the MTMA is kept in the range of 50° C. to 100° C. [6" id="US-20010006835-A1-CLM-00006] 6. The method of claim 5 , wherein the temperature of a supply-line from the MTMA source vessel to the reaction chamber is kept in the range of 70° C. to 180° C. [7" id="US-20010006835-A1-CLM-00007] 7. The method of claim 1 , wherein the oxygen source is selected from the group consisting of H2O, O2, N2O, O3. [8" id="US-20010006835-A1-CLM-00008] 8. The method of claim 7 , wherein the step (d) is carried out for 0.1 to 3 seconds. [9" id="US-20010006835-A1-CLM-00009] 9. The method of claim 1 , wherein the aluminum oxide is deposited on condition that the temperature of the reaction chamber ranges from 200° C. to 450° C. and the pressure is approximately 300 mTorr. [10" id="US-20010006835-A1-CLM-00010] 10. A method for manufacturing a semiconductor device, comprising the steps of: (a) preparing an active matrix provided with a substrate, isolation regions, gate line, gate oxide and a first insulating layer; (b) forming a buffer layer and a first conductive layer on the active matrix; (c) forming a dielectric layer of aluminum oxide (Al2O3) on the first conductive layer by using an ALD method, MTMA being used as aluminum source material; (d) forming a second conductive layer on the dielectric layer and patterning the second conductive layer, the dielectric layer, the first conductive layer and the buffer layer, thereby obtaining a capacitor structure; (e) forming a hydrogen barrier layer on the capacitor structure; (f) forming a bit line and a local interconnection after depositing a second insulating layer; and (g) forming a passivation layer on the bit line, the local interconnection and the second insulating layer. [11" id="US-20010006835-A1-CLM-00011] 11. The method of claim 10 , wherein the gate oxide is made of aluminum oxide processed by an ALD method and MTMA is used as aluminum source material. [12" id="US-20010006835-A1-CLM-00012] 12. The method of claim 10 , wherein the hydrogen barrier layer is made of aluminum oxide processed by an ALD method and MTMA is used as aluminum source material. [13" id="US-20010006835-A1-CLM-00013] 13. The method of claim 10 , wherein after the step (c), there is a step of annealing the dielectric layer for densification. [14" id="US-20010006835-A1-CLM-00014] 14. The method of claim 13 , wherein the step of annealing the dielectric layer is carried out at a temperature ranging from 750° C. to 850° C. [15" id="US-20010006835-A1-CLM-00015] 15. The method of claim 11 , wherein an N2 purging time for forming the aluminum oxide as the gate oxide is approximately 5 to 10 seconds. [16" id="US-20010006835-A1-CLM-00016] 16. The method of claim 13 , wherein the aluminum oxide as the hydrogen barrier layer is formed to a thickness ranging from 60Å to 200Å.
类似技术:
公开号 | 公开日 | 专利标题 US6589886B2|2003-07-08|Method for manufacturing aluminum oxide film for use in a semiconductor device US6509601B1|2003-01-21|Semiconductor memory device having capacitor protection layer and method for manufacturing the same US6849505B2|2005-02-01|Semiconductor device and method for fabricating the same US6723598B2|2004-04-20|Method for manufacturing aluminum oxide films for use in semiconductor devices US5702970A|1997-12-30|Method for fabricating a capacitor of a semiconductor device US7309889B2|2007-12-18|Constructions comprising perovskite-type dielectric US20040063275A1|2004-04-01|Capacitor of a semiconductor memory device and method of forming the seme US20030148605A1|2003-08-07|Method of forming an oxidation-resistant TiSiN film US6340622B1|2002-01-22|Method for fabricating capacitors of semiconductor device JP2001111000A|2001-04-20|Semiconductor element and manufacturing method thereof US20060214204A1|2006-09-28|Ferroelectric structures and devices including upper/lower electrodes of different metals and methods of forming the same US20010005612A1|2001-06-28|Method for forming a capacitor using tantalum nitride as a capacitor dielectric US6486022B2|2002-11-26|Method of fabricating capacitors KR20040076447A|2004-09-01|Method for forming a capacitor in a semiconductor device US6376299B1|2002-04-23|Capacitor for semiconductor memory device and method of manufacturing the same US6525364B1|2003-02-25|Capacitor for semiconductor memory device and method of manufacturing the same US6682974B2|2004-01-27|Fabricating capacitor of semiconductor device US6410400B1|2002-06-25|Method of manufacturing Ta2O5capacitor using Ta2O5thin film as dielectric layer KR100464650B1|2005-01-03|Capacitor of semiconductor device having dual dielectric layer structure and method for fabricating the same US6541330B1|2003-04-01|Capacitor for semiconductor memory device and method of manufacturing the same US6777740B2|2004-08-17|Capacitor for semiconductor memory device and method of manufacturing the same JP2001127258A|2001-05-11|Semiconductor device and manufacturing method therefor US6635524B2|2003-10-21|Method for fabricating capacitor of semiconductor memory device US7608517B2|2009-10-27|Method for forming capacitor of semiconductor device KR100406546B1|2003-11-22|Method for fabricating capacitor
同族专利:
公开号 | 公开日 TW480622B|2002-03-21| JP2001244263A|2001-09-07| US6589886B2|2003-07-08| KR20010063478A|2001-07-09| KR100323874B1|2002-02-16|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题 WO2002031875A2|2000-10-10|2002-04-18|Asm America, Inc.|Dielectric interface films and methods therefor| WO2004011693A1|2002-07-29|2004-02-05|Micron Technology, Inc.|Atomic deposition layer methods| EP1394848A2|2002-08-30|2004-03-03|Infineon Technologies AG|Etch process and etch stop layer for manufacturing of semiconductor wafers| US6821862B2|2000-06-27|2004-11-23|Samsung Electronics Co., Ltd.|Methods of manufacturing integrated circuit devices that include a metal oxide layer disposed on another layer to protect the other layer from diffusion of impurities and integrated circuit devices manufactured using same| US20050255663A1|2004-05-13|2005-11-17|Katsuaki Natori|Semiconductor device and method of manufacturing the same| US7160578B2|2004-03-10|2007-01-09|Pilkington North America|Method for depositing aluminum oxide coatings on flat glass| US20080067590A1|2006-05-12|2008-03-20|Renesas Technology Corp.|Semiconductor device and manufacturing method of the same| US20130237030A1|2007-10-30|2013-09-12|Spansion Llc|Metal-insulator-metaldevice and method of formation thereof| US20150147482A1|2013-11-25|2015-05-28|Lam Research Corporation|Chamber undercoat preparation method for low temperature ald films| CN106567053A|2015-10-09|2017-04-19|中国科学院微电子研究所|Method for preparing titanium-aluminum alloy film| US9828672B2|2015-03-26|2017-11-28|Lam Research Corporation|Minimizing radical recombination using ALD silicon oxide surface coating with intermittent restoration plasma| US10023956B2|2015-04-09|2018-07-17|Lam Research Corporation|Eliminating first wafer metal contamination effect in high density plasma chemical vapor deposition systems| US10211099B2|2016-12-19|2019-02-19|Lam Research Corporation|Chamber conditioning for remote plasma process| US20200090924A1|2018-09-14|2020-03-19|Applied Materials, Inc.|Selective aluminum oxide film deposition| CN111128863A|2018-10-31|2020-05-08|台湾积体电路制造股份有限公司|Semiconductor interconnect structure and method of forming a semiconductor structure| US10760158B2|2017-12-15|2020-09-01|Lam Research Corporation|Ex situ coating of chamber components for semiconductor processing|KR100269306B1|1997-07-31|2000-10-16|윤종용|Integrate circuit device having buffer layer containing metal oxide stabilized by low temperature treatment and fabricating method thereof| US6305314B1|1999-03-11|2001-10-23|Genvs, Inc.|Apparatus and concept for minimizing parasitic chemical vapor deposition during atomic layer deposition| US6255122B1|1999-04-27|2001-07-03|International Business Machines Corporation|Amorphous dielectric capacitors on silicon| US6780704B1|1999-12-03|2004-08-24|Asm International Nv|Conformal thin films over textured capacitor electrodes| KR100385946B1|1999-12-08|2003-06-02|삼성전자주식회사|Method for forming a metal layer by an atomic layer deposition and a semiconductor device with the metal layer as a barrier metal layer, an upper electrode, or a lower electrode of capacitor| KR20020004539A|2000-07-06|2002-01-16|박종섭|Method for forming FeRAM capable of preventing hydrogen diffusion|KR100481848B1|1998-12-15|2006-05-16|삼성전자주식회사|Manufacturing method of dielectric film without chemical defect| US9255329B2|2000-12-06|2016-02-09|Novellus Systems, Inc.|Modulated ion-induced atomic layer deposition | US6627268B1|2001-05-03|2003-09-30|Novellus Systems, Inc.|Sequential ion, UV, and electron induced chemical vapor deposition| JP3466174B2|2001-09-27|2003-11-10|沖電気工業株式会社|Semiconductor device and manufacturing method thereof| US20030224536A1|2002-06-04|2003-12-04|Andreas Hilliger|Contact formation| US6890596B2|2002-08-15|2005-05-10|Micron Technology, Inc.|Deposition methods| US6753271B2|2002-08-15|2004-06-22|Micron Technology, Inc.|Atomic layer deposition methods| US6673701B1|2002-08-27|2004-01-06|Micron Technology, Inc.|Atomic layer deposition methods| KR100721856B1|2004-02-06|2007-05-28|김상관|Power Supply for Detection Trouble of Light Emitting DiodeLED Signal Lamp| JP4284228B2|2004-04-19|2009-06-24|株式会社東芝|Manufacturing method of semiconductor device| KR100695511B1|2004-06-07|2007-03-15|주식회사 하이닉스반도체|Method for manufacturing the aluminium oxide thin film of semiconductor devices using the atomic layer deposition| US20050276922A1|2004-06-10|2005-12-15|Henry Bernhardt|Method of forming thin dielectric layers| JP4946145B2|2006-04-13|2012-06-06|富士通セミコンダクター株式会社|Manufacturing method of ferroelectric memory| US8053372B1|2006-09-12|2011-11-08|Novellus Systems, Inc.|Method of reducing plasma stabilization time in a cyclic deposition process| US7871678B1|2006-09-12|2011-01-18|Novellus Systems, Inc.|Method of increasing the reactivity of a precursor in a cyclic deposition process| KR100829821B1|2006-10-25|2008-05-19|주식회사 아이피에스|Method of depositing thin film| JP5344873B2|2008-08-28|2013-11-20|三菱電機株式会社|Method for manufacturing silicon carbide semiconductor device| US8747964B2|2010-11-04|2014-06-10|Novellus Systems, Inc.|Ion-induced atomic layer deposition of tantalum| JP6874586B2|2017-08-09|2021-05-19|富士通株式会社|Semiconductor devices and methods for manufacturing semiconductor devices| US10707089B2|2018-03-27|2020-07-07|Texas Instruments Incorporated|Dry etch process landing on metal oxide etch stop layer over metal layer and structure formed thereby|
法律状态:
2001-03-12| AS| Assignment|Owner name: HYUNDAI ELECTRONICS INDUSTRIES CO., LTD., KOREA, R Free format text: ASSIGNMENT OF ASSIGNORS INTEREST;ASSIGNORS:KIM, MIN-SOO;KIM, KYONG-MIN;LIM, CHAN;AND OTHERS;REEL/FRAME:011576/0669 Effective date: 20001220 | 2003-06-19| STCF| Information on status: patent grant|Free format text: PATENTED CASE | 2006-12-18| FPAY| Fee payment|Year of fee payment: 4 | 2010-12-02| FPAY| Fee payment|Year of fee payment: 8 | 2014-12-29| FPAY| Fee payment|Year of fee payment: 12 |
优先权:
[返回顶部]
申请号 | 申请日 | 专利标题 KR1019990060563A|KR100323874B1|1999-12-22|1999-12-22|Method of forming an aluminum oxide film in a semiconductor device| KR1999-60563||1999-12-22|| KR99-60563||1999-12-22|| 相关专利
Sulfonates, polymers, resist compositions and patterning process
Washing machine
Washing machine
Device for fixture finishing and tension adjusting of membrane
Structure for Equipping Band in a Plane Cathode Ray Tube
Process for preparation of 7 alpha-carboxyl 9, 11-epoxy steroids and intermediates useful therein an
国家/地区
|