![]() Blow molded container with memory shrink closure attachment and method of making the same
专利摘要:
A blow molded, bi-axially oriented plastic canister or container has a generally cylindrical body, a bottom, and a tapering upper portion, which terminates at a wide mouth or opening surrounded by a radially outwardly directed annular flange having an inwardly facing corner. A generally disc-shaped closure insert having a circumferential rim and a dispensing outlet is placed across the opening such that the closure rim is generally fitted into the corner of the annular flange. Heat or some other form of energy is applied to the entirety of the annular flange, which in response shrinks to tightly conform to and engage the closure rim, forming a circumferential seal. The dispensing outlet may be provided with an outlet closure, such as a screw cap or the like. Also, a sealant may be disposed between the annular flange and the closure rim before the heat is applied in order to form an enhanced seal. Furthermore, mechanical devices may be used to shape the flange during or after heating to further enhance the rim-flange seal or to provide additional sealing configurations. 公开号:US20010000373A1 申请号:US09/739,177 申请日:2000-12-18 公开日:2001-04-26 发明作者:Martin Beck 申请人:Beck Martin H.; IPC主号:B29C65-66
专利说明:
[1] 1. This invention relates to blow molded plastic containers, and more particularly, though not exclusively, to closures for blow molded hot fill plastic containers. DEFINITION [2] 2. Material memory, as used herein, is the propensity of materials, particularly plastics (especially polyesters, e.g. PET), to return to a previous shape or size upon the relief of internal stresses, produced, for example, by molecular orientation when blow molding an article from a preform, the relief usually being provided by the application of energy to heat the material to a stress relieving temperature. BACKGROUND OF THE INVENTION [3] 3. Bottles or containers made from polyesters, usually polyethylene terephthalate (PET) or other plastics, are well known, and provide a lighter, more economical, and typically stronger alternative to older, more traditional glass or metal containers. [4] 4. PET containers are typically manufactured using plastic preforms in conjunction with a blow molding process. Such containers come in all shapes and sizes, may be wide-mouthed or narrow-mouthed, and are provided with numerous types of closures including, for example, screw-on closures and snap-on closures. Frequently, the containers' necks will be provided with complementary attachment means (neck finishes) for facilitating the attachment of the respective types of closures. [5] 5. Wide mouth blow molded containers are often outfitted with screw-thread neck finishes via an injection stretch blow mold process, the neck finish being made during the initial injection molding process of the preform. One problem with wide mouth neck finishes and closures is that extra manufacturing steps may be necessary to ensure the neck area is as strong as the rest of the container. This is because during the stretch blow molding process the body of the container is biaxially oriented (thus increasing its relative strength), while the neck area is not (because the injection molding process does not significantly orient the plastic). Intermediate heat treatment steps and the like may be necessary to ensure proper strength throughout the container. [6] 6. Alternatively, wide mouth containers may be provided with a simpler neck finish once the blow molding process is completed by mechanically manipulating the neck area. For example, the neck rim may be formed into a circumferential, rolled lip, onto which a complementary closure is simply snapped into place. Such a closure, though, may not always provide an adequate seal, and it may not be desirable to have such a wide product dispensing opening in the container once the closure is removed. SUMMARY OF THE INVENTION [7] 7. Wherefore, it is an object of the present invention to overcome the aforementioned problems and drawbacks associated with the prior art designs by providing a novel and advantageous closure for wide mouth, plastic blow molded containers. [8] 8. Another object of the invention is to provide a method for closing wide mouth containers which allows for a variety of closure types. [9] 9. Another object of the present invention is to provide a wide mouth blow molded container having a permanently secured wide mouth closure. [10] 10. Yet another object of the invention is to provide a simpler and more economic method of closing and producing wide mouth containers having uniform or near uniform container strength without the necessity of many additional manufacturing steps. [11] 11. Another object of the present invention is to provide a wide mouth blow molded container wherein the closure may be a compound closure having multiple and/or alternative closure parts. [12] 12. Yet another object of the invention is to provide a wide mouth container closure having an enhanced seal, and the potential to provide numerous types of seals. [13] 13. The present invention provides, in combination, a container and closure comprising: a container defining an opening and having at least one portion with a material memory; and a closure insert defining a closure periphery, the closure insert being secured in the container by material shrinkage produced by relief of stresses in the material memory container portion to conform that portion to the closure periphery. [14] 14. The present invention also provides a method of closing a container comprising the steps of: providing a container defining an opening and having at least one portion having a material memory; providing a closure defining a closure periphery; positioning the closure in the container with at least a portion of the closure periphery being proximate the material memory portion; and heating the material memory portion sufficient to cause the material memory portion to shrink and thereby engage and conform to the closure periphery. [15] 15. The present invention also provides a method of manufacturing a container having a closure, the method comprising the steps of: blow molding a container comprising a body and an accommodation element from a thermoplastic material, the accommodation element comprising an annular flange having a horizontal, radially extending portion and a vertical, axially oriented portion extending upwards from an edge thereof, the horizontal and vertical portions defining an inwardly facing, circumferential corner, and the material of the body and at least a portion of the accommodation element proximate the body being biaxially oriented via the blow molding process; trimming and removing a portion of the accommodation element above the vertical portion of the annular flange in order to provide a container opening defined by the annular flange; providing a closure insert having a closure periphery; positioning the closure insert across the container opening such that at least a portion of the closure periphery rests in the corner of the annular flange; and heating the annular flange sufficient to shrink the annular flange to engage and conform to the portion of the closure periphery resting in the corner of the annular flange. [16] 16. The present invention also provides a method of closing a container comprising the steps of: providing a container having at least one generally planar portion, the container defining an opening, and the container having at least one flap integral with the at least one generally planar portion, the at least one flap extending beyond the opening, and the container having at least one portion having a longitudinal material memory, the at least one material memory portion being proximate a junction between the at least one flap and the at least one generally planar portion; and heating the material memory portion sufficient to cause the material memory portion to longitudinally contract, the at least one flap thereby generally folding over to at least partially cover the opening. [17] 17. The present invention discloses a blow molded, biaxially oriented plastic canister or container having a generally cylindrical body, a bottom, and a tapering upper portion, which terminates at a wide mouth or opening surrounded by a radially outwardly directed annular flange. The annular flange includes a horizontal, disc-like portion and a vertical, cylindrical portion extending up from the horizontal portion. A generally disc-shaped closure insert having a circumferential rim and a dispensing outlet is placed across the opening such that the closure rim is generally fitted into a corner formed by the horizontal and vertical portions of the annular flange. [18] 18. Heat or some other form of radiant energy is applied to the entirety of the annular flange, which, having been at least radially or circumferentially oriented during the blow molding process, shrinks in response to tightly conform to and engage the closure rim, forming a circumferential seal. The dispensing outlet may be provided with an outlet closure, such as a screw cap or the like, depending on the configuration of the provided dispensing outlet. Also, a sealing gasket or the like may be disposed between the annular flange and the closure rim before the heat is applied in order to form an enhanced seal. Furthermore, mechanical devices may be used to shape the flange during or after heating to further enhance the rim-flange seal or to provide additional sealing configurations. BRIEF DESCRIPTION OF THE DRAWINGS [19] 19. The invention will now be described, by way of example, with reference to the accompanying drawings, in which: [20] 20.FIG. 1 is an elevational perspective view of a clear plastic blow molded container having a memory shrink closure attachment according to the present invention; [21] 21.FIG. 2 is a cross-sectional view (with detail) of the container of FIG. 1 taken across section line 2—2; [22] 22.FIG. 3 is a cross-sectional view of the container during an intermediate manufacturing step, as known in the prior art; [23] 23.FIG. 4 is a cross-sectional view of a preform used to make the plastic container, as known in the prior art; [24] 24.FIG. 5 is a cross-sectional detail view of the manufacturing process of the closure according to the present invention; [25] 25.FIG. 6 is a cross-sectional detail view of the container of FIG. 2 showing the placement of an optional sealant; [26] 26.FIG. 7 is a cross-sectional detail view of the container of FIG. 2 showing an additional embodiment of the present invention; [27] 27.FIG. 8 is a cross-sectional detail view of the container of FIG. 2 having an alternative rim and sealing configuration; [28] 28.FIG. 9 shows a cross-sectional view of an alternative configuration for a dispensing outlet and closure rim, further including a closure cap; [29] 29.FIG. 10A is a fragmentary cross-sectional view illustrating one of the inventive elements of the present invention and a first step in exemplary embodiment thereof; [30] 30.FIG. 10B is a fragmentary cross-sectional view showing a second step in the exemplary embodiment of the present invention; [31] 31.FIG. 11 is a perspective view illustrating one of the inventive elements of the present invention and an additional embodiment thereof; [32] 32.FIG. 12A is a perspective view of another embodiment of the present invention, similar to the embodiment of FIG. 11, in a pre-closure state, and illustrating an additional inventive element of the present invention;; [33] 33.FIG. 12B is a perspective view of the embodiment of FIG. 12A in a post-closure state; [34] 34.FIG. 13 is a fragmentary cross-sectional view of an additional embodiment of the present invention using a flange-less container; and [35] 35.FIG. 14 is a fragmentary cross-sectional view of an additional embodiment of the present invention provided with a screw-on closure. DESCRIPTION OF THE PREFERRED EMBODIMENTS [36] 36. Turning to FIGS. 1-5, a detailed description of further embodiments of the present invention will now be provided. [37] 37. In FIG. 1, the container 10 is a blow molded, wide mouth plastic container having a generally cylindrical body 12 and a bottom 14. The bottom 14 may be of the modified champagne type so as to resist internal pressures. An upper part 16 of the body 12 tapers radially inwardly and axially upwardly, and terminates in a wide mouth or opening 18. As best seen in FIGS. 3 and 5, the opening 18 is surrounded by a radially outwardly directed annular flange 20 which initially includes a horizontal, disc-like portion 22 and a vertical, cylindrical portion 24 extending up from the horizontal portion to form a circumferential corner 26. [38] 38. This container and a method for making the same is disclosed in U.S. Pat. No. 4,576,843 (the '843 patent), to Beck et al. In the '843 patent the wide mouth container 10 is formed from a small diameter preform 30 (see FIG. 4) as is customarily utilized in the blow molding of plastic containers, with the preform being of a materially lesser length than that of the resultant container. As shown in FIG. 3, in order to obtain the necessary biaxial orientation of the thermoplastic material throughout the container 10, an intermediate article of manufacture is produced. This is essentially the container 10 with an additional accommodation element portion 32, the accommodation element 32 being severed or trimmed from the container near line L and becoming reusable scrap. The resulting wide mouthed container 10 is thus completely biaxially oriented, and has the annular flange 20 once the accommodation element is removed. [39] 39. In addition, in the generally cylindrical container 10 as shown, the outward radial expansion of the preform 30 during blow molding results in the container being radially inwardly internally stressed. That is, subsequent the blow molding process, the container material is molecularly oriented to offset a desire to contract circumferentially inward to its previous state. If energy is subsequently applied to a portion of the container material, the internal stresses will be relieved and that portion will actually contract circumferentially inwards. As defined above, this characteristic is known as material memory. Also, it should be noted that in the case of PET and most other plastics commonly used for plastic containers, once the material has returned to its original state according to its material memory, its morphology has typically been altered to a state of increased crystallinity. Thus, the material will no longer be effected by subsequent applications of energy. In this sense, the material is permanently deformed. [40] 40. Once the container 10 has been blow molded and trimmed, it is ready to receive the closure insert 40. The closure insert 40, as best seen in FIG. 1, is generally disc-shaped and has a circumferential closure rim 42 (the rim defining a periphery of the closure insert), the outer edge of which is typically rounded. The closure insert 40 also includes a dispensing outlet 44, which may be a hole or void disposed near the center of the closure insert 40 as shown in FIG. 1, though it may be any shape or size depending on the particular application. The dispensing outlet 44 may have an outlet rim 46, which can be configured to engage a snap-on closure cap, a screw-on closure, a non-resealable closure or the like, with or without further tamper-proof features such as sealing discs and tear off skirts. One preferred outlet rim/closure cap configuration is shown in FIG. 9, as discussed below. [41] 41. The closure insert 40 is preferably made from a metal such as aluminum or steel, but may also be made from plastic, cardboard, plastic lined metal, etc. Because the manufacture of such a closure insert is known to those of ordinary skill in the art, further detail will not be provided herein. [42] 42.FIG. 5 shows the first steps in the process of attaching the closure insert 40 to the wide mouth container 10. The closure insert 40 is first placed across the opening 18 such that the closure rim 42 rests in the corner 26 between the horizontal flange portion 22 and the vertical flange portion 24. Next, a heater 50 (or some other energy source) is used to apply heat to the flange 20 as indicated by the arrows in FIG. 5. This causes the plastic material, which retains a material memory of its previous, preform configuration, as discussed above, to shrink inwards. The flange thus contacts, wraps around, and conforms to the closure rim 42, providing a tight seal (as best seen in FIG. 2). Ideally the heater 50 is shaped (for example, as a hollow cylinder) so that the entirety of the flange 20 may be heated at the same time. [43] 43. As mentioned above, once the material of the flange 20 has contracted around the closure insert, it is in a state of permanent deformation. Absent the application of catastrophic force (mechanical cutting, fire, etc.), the closure insert 40 is thus permanently affixed to the container. However, it should be remembered that containers with removable closures may be provided according to the present invention, as described below. [44] 44. Referring now to FIG. 6, a sealant 52 may be disposed between the closure rim 42 and the annular flange 20 in order to provide an enhanced circumferential seal. The sealant 52 may be a foam, plastic or rubber gasket, or some form of adhesive, hardening sealant, or the like. During the manufacturing process, the sealant 52 is placed into the flange corner 26 before the closure insert 40 is positioned across the opening 18. If a liquid or semi-solid adhesive or the like is used as the sealant 52, it may be sprayed or squirted into the corner 26 via a dispensing nozzle or some other applicator (not shown). Once the sealant 52 is in place, the closure insert 40 is put into place, and the flange 20 heated as described above. Alternatively, the closure rim 42 may be provided with sealant 52 prior to placement, and the entirety placed into the flange corner 26. [45] 45.FIG. 7 shows an additional embodiment of the present invention wherein the annular flange 20 includes a flange extension 56 that extends fully over and beyond the closure rim 42. Such a feature provides an enhanced, stronger seal between the container 10 and closure insert 40. Since the flange extension 56 may not strictly conform to the shape of the closure insert (around the area where the closure rim 42 meets the closure insert 40 proper), a pressure tool 58 may be used to shape the flange extension 56 via a force applied in a direction as indicated by the arrow in FIG. 7. The pressure tool 58 may be a circular or disc-shaped press, in which case the direction of the force would be straight down. A sealant 52 (not shown in FIG. 7) may also be provided to enhance the seal of this embodiment. [46] 46. An additional embodiment of the present invention is shown in FIG. 8. Here, the closure rim 42 is provided with an outwardly facing, circumferential groove 60. During or after heating of the flange 20, a second pressure tool 62 (preferably provided as one or more shaped rollers) may be used to press the flange 20 into the rim groove 60 via a force applied in a direction as indicated by the arrow in FIG. 8. Again, a sealant 52 may be used with the configuration of this embodiment. [47] 47. Turning now to FIG. 9, a preferred embodiment of the dispensing outlet and outlet rim is shown in cross-section. Here, the outlet rim 46 is formed via an initially upwardly extending curl of the closure insert 40 around the dispensing outlet 44. Such a curl can be manufactured by a metal forming tool, for example, as known to those with skill in the art. Additionally, a closure cap 64, provided with features dimensioned to tightly engage the outlet rim 46 (a lower circumferential sealing lip 66 for example), may be provided to disengagingly seal the dispensing outlet 44. The closure cap 64 may be provided with a pull tab 68 to facilitate removal. Of course, the type of closure cap provided will depend on the particular application. For example, if the container is to be used to hold spices, the closure cap may have shaker/sifter holes disposed therein. [48] 48. Although the present invention has been illustrated for use with a container having a particular configuration, one of ordinary skill in the art will appreciate thatthe present invention could be used with other containers without departing from the spirit and scope of the invention. For example, containers without tapering top portions 16 could be used, or containers having wider mouths, or containers having different shapes or sizes. [49] 49. Also, although the present invention has been shown in use with a container having an annular flange with a horizontal portion and a vertical portion, one of ordinary skill in the art will appreciate that the closure attachment could be used on a container with only a horizontal flange by providing a pressure or guidance tool that would guide the flange over the closure rim during heating/shrinking. [50] 50. Also, although the present invention has been illustrated in conjunction with a generally disc-shaped closure insert, one of ordinary skill in the art will appreciate that any shaped closure insert could be used without departing from the spirit and scope of the invention, provided that the closure insert has at least some sort of rim portion. It should also be appreciated that the closure rim does not have to be any one particular shape (as was shown in the embodiment of FIG. 8, for example). [51] 51. Turning now to FIGS. 10A and 10B, one of the inventive elements of the present invention and a first embodiment thereof shall be described with reference to an example. [52] 52. In FIG. 10A, a container orother object 10 is at least partially made from a material capable of retaining a material memory, such as PET. The container 10 has at least one portion 11 that has been stressed or strained such that the strained portion 11 is oriented and therefore retains a memory of its previous, unstrained state. The stress or strain need not only be applied via molecular orientation (at least radial or circumferential and usually biaxial and radial orientation) during stretch blow molding, but may be imparted by another stretching process, the application of some other mechanical force, or the application of energy, as appropriate to the application and type of material used. [53] 53. In FIG. 10A, a closure insert or other member 40 having a rim portion 42 is placed in contact or proximate the container 10 having at least the one strained circumferential portion orarea 11. Subsequent an application of energy to heat the area 11, the strained portion 11 contracts (i.e. tends to returns to its previous state), and engages the rim portion 42, as shown in FIG. 10B. Of course, the rim should be positioned such that the contracting strained portion 11 encounters the rim before the strained portion fully returns to its original, pre-strain condition. If the member 40 is a closure, the container 10 may then be trimmed proximate line L2. Alternatively, it is possible to provide a removable closure by cutting the container proximate line L4, although this would result in there no longer being a permanent, tight seal. Finally, the closure 40 may be disposed proximate a termination of the container 10 before attachment, as illustrated by line L3 in FIG. 10A. [54] 54. It should be appreciated that this technique can be used to provide a seal between any container having at least one appropriately oriented portion having a material memory and a closure or other member having any shape. One example of this is shown in FIG. 11, where a cross member 5 is disposed between two opposing walls 6 of a container having, e.g. a square cross-section, each having a strained area or portion 11. If the cross member 5 is a closure, the walls 6 would terminate or be trimmed proximate a plane P. It will be appreciated that only three of four walls defining the containers are shown in FIG. 11 and that other cross-sections having planar or curved walls are contemplated by the present invention. [55] 55.FIGS. 12A and 12B show an additional embodiment of the present invention. Here, the square container of FIG. 11 is provided without the cross member 5. Two corner segments are cut at 70, effectively providing three rectangular flaps 72. In addition, at least the areas 11 proximate the junctions between the flaps and the container proper have laterally directed material memories (e.g. as provided by stretch molding). Energy is subsequently applied to the material memory areas 11, which tend to bend inwardly in response so that the flaps 72 generally fold over, as shown in FIG. 12B. To open the flaps, a user simply pulls upwards on leading edges 74, essentially overcoming the otherwise permanently folded flaps via mechanical force. Although this configuration would not provide a water tight seal, it would be useful for containers to store certain types of goods, e.g. a square tube container for tennis balls. [56] 56. It should be appreciated that for an actual container a fourth wall would be provided, preferably along with a fourth flap. Of course, it would be possible to provide an effective closure with only a single flap, or more than fourflaps (for example, a turret-shaped configuration), depending on the particular application. Also, the flaps could be any shape, e.g. rounded, and the material memory folding process could be facilitated or further controlled by using mechanical presses, guides, or the like. [57] 57. Turning now to FIG. 13, an additional embodiment is shown wherein the container 10 is provided without an annular flange 20. This is accomplished by cutting the intermediate article of manufacture as shown in FIG. 3 proximate a line L′. In addition, a pre-molded closure 40 is provided. The closure 40 comprises a generally cylindrical body 76 having a product dispensing opening 77 disposed longitudinally therethrough, an annular flange 78 extending around the top of the body 76, and an outwardly facing circumferential groove 79 disposed about a lower portion of the body 76 below the annular flange 78. For assembly, the closure 40 is inserted into the container opening 18, and is supported by the annular flange abutting a top rim of the container 10. The closure 40 is preferably dimensioned to tightly fit within the opening. Then the container is heated and mechanically pressed proximate a stressed/oriented area 11, as was illustrated in FIG. 8. This provides a permanent sealing closure between the closure 40 and the container 10, which may be enhanced by using sealants, gaskets, or the like, as discussed above with respect to other embodiments. [58] 58. Finally, FIG. 14 shows a version of the embodiment of FIG. 13 having a removable, pre-formed, screw threaded closure 40. Here, the screw thread on closure 40 has a helical form 80 extending circumferentially around the closure 40. The term “screw thread,” as used herein, refers to a continuous or interrupted (by one or more spaces) helical thread, as known to those with skill in the art, to effectuate increased manufacturing tolerances during molding and the like. [59] 59. The closure is placed into the mouth opening of a flange-less container 10, as was shown in FIG. 13 (for a flanged container as described above). A complementary shaped heating unit 82 or the like is then used to heat the container 10 proximate the thread portions 80 so that the container radially contracts (shrinks) to engage the threads. Once the heated material has cooled sufficiently to form a permanent deformation, the closure 40 may be removed, for example, by gripping the annular flange 78 and twisting appropriately. Appropriate container seal features may be provided. [60] 60. The engaging threads could be provided with an intermediate seal layer fracturable to allow removal for access to the container. [61] 61. Since certain changes may be made in the above described memory shrink closure attachment, without departing from the spirit and scope of the invention herein involved, it is intended that all of the subject matter of the above description or shown in the accompanying drawings shall be interpreted merely as examples illustrating the inventive concept herein and shall not be construed as limiting the invention. LIST OF ELEMENTS 5 cross member 6 walls 10 container generally 11 strained portion of container 12 container body 14 container bottom 16 container top portion 18 container mouth/opening 20 annular flange 22 annular flange horizontal portion 24 annular flange vertical portion 26 annular flange corner 30 preform (FIG. 4) 32 accommodation element (FIG. 5) 40 closure insert 42 closure rim 44 dispensing outlet 46 outlet rim 50 heater/radiant energy source 52 sealant 56 flange extension 58 pressure tool 60 circumferential closure rim groove 62 second pressure tool 64 closure cap 66 closure cap lower sealing lip 68 closure cap pull tab 70 cut corner segments 72 flaps 74 leading edges of flaps 76 cylindrical body of flanged closure 77 dispensing opening 78 annular flange of closure 79 circumferential groove 80 helical form or thread portions 82 heating unit
权利要求:
Claims (25) [1" id="US-20010000373-A1-CLM-00001] 1. In combination, a container and closure comprising: a container defining an opening and having at least one portion with a material memory; and a closure insert defining a closure periphery, the closure insert being secured in the container by material shrinkage produced by relief of stresses in the material memory-container portion to conform that portion to the closure periphery. [2" id="US-20010000373-A1-CLM-00002] 2. The container and closure of claim 1 wherein the at least one material memory portion is proximate the opening and wherein the closure insert is disposed in the container proximate the opening. [3" id="US-20010000373-A1-CLM-00003] 3. The container and closure of claim 2 wherein the material memory portion is an annular flange defining the opening, and the closure periphery engages at least a portion of the annular flange via the annular flange having been shrunk to generally conform to the shape of the closure periphery. [4" id="US-20010000373-A1-CLM-00004] 4. The container and closure of claim 3 wherein the annular flange comprises, in addition to the portion engaging the closure periphery, a generally horizontal portion further supporting the closure. [5" id="US-20010000373-A1-CLM-00005] 5. The container and closure of claim 3 wherein an outwardly facing circumferential groove is disposed in the closure periphery, a portion of the annular flange engaging and substantially conforming to the shape of the groove subsequent to the material shrinkage and a mechanical pressing. [6" id="US-20010000373-A1-CLM-00006] 6. The container and closure of claim 3 wherein the annular flange further includes a flange extension that afterthe material shrinkage extends fully over and beyond the closure periphery towards a center of the closure, the flange extension conforming to the shape of the closure subsequent the application of a mechanical force. [7" id="US-20010000373-A1-CLM-00007] 7. The container and closure of claim 2 wherein the material memory portion is at least proximate a circumferential rim defining the opening, and wherein the closure has an annular flange extending around the closure, the annular flange being dimensioned larger than the opening for abutting engagement with the rim, and the closure having an outwardly facing circumferential groove below the annular flange, the material memory portion of the container engaging and substantially conforming to the shape of the groove subsequent to material shrinkage and a mechanical pressing. [8" id="US-20010000373-A1-CLM-00008] 8. The container and closure of claim 2 wherein the material memory portion is at least proximate a circumferential rim defining the opening, and wherein the closure has an annular flange extending around the closure, the annular flange being dimensioned larger than the opening for abutting engagement with the rim, and the closure having an outwardly facing helical thread disposed below the annular flange, the material memory portion of the container engaging and substantially conforming to the shape of the helical thread or thread portions subsequent to material shrinkage and a mechanical pressing. [9" id="US-20010000373-A1-CLM-00009] 9. The container and closure of claim 1 wherein the closure periphery is a rim having at least an outer edge of which is substantially rounded. [10" id="US-20010000373-A1-CLM-00010] 10. The container and closure of claim 1 wherein a sealant is disposed between at least a portion of the closure periphery and at least a portion of the material memory container portion. [11" id="US-20010000373-A1-CLM-00011] 11. The container and closure of claim 1 wherein a dispensing outlet is disposed in the closure insert. [12" id="US-20010000373-A1-CLM-00012] 12. The container and closure of claim 11 further comprising an outlet rim provided integral to the closure around the dispensing outlet. [13" id="US-20010000373-A1-CLM-00013] 13. The container and closure of claim 12 further comprising a closure cap, the outlet rim being dimensioned to sealingly engage the closure cap. [14" id="US-20010000373-A1-CLM-00014] 14. The container and closure of claim 1 wherein the container is a stretch blow molded plastic container, and the material memory portion is provided via the plastic having been at least radially oriented during the blow molding process. [15" id="US-20010000373-A1-CLM-00015] 15. The container of claim 14 wherein the plastic has been biaxially oriented. [16" id="US-20010000373-A1-CLM-00016] 16. The container of claim 1 wherein the closure insert is permanently secured in the container by the material memory. [17" id="US-20010000373-A1-CLM-00017] 17. The container and closure of claim 1 wherein the closure insert is permanently secured in the container via the morphology of the material memory portion having been altered to a state of increased crystallinity as a result of the material shrinkage. [18" id="US-20010000373-A1-CLM-00018] 18. A method of closing a container comprising the steps of: providing a container defining an opening and having at least one portion having a material memory; providing a closure defining a closure periphery; positioning the closure in the containerwith at least a portion of the closure periphery being proximate the material memory portion; and heating the material memory portion sufficient to cause the material memory portion to shrink and thereby engage and conform to the closure periphery. [19" id="US-20010000373-A1-CLM-00019] 19. The method of claim 18 further comprising the step, before the step of heating, of providing a sealant between at least a portion of the material memory portion and the closure periphery whereby once the material memory portion is shrunk via the step of heating an enhanced seal between the container and closure periphery is realized. [20" id="US-20010000373-A1-CLM-00020] 20. The method of claim 18 wherein the material memory portion is proximate the opening, and wherein the step of positioning comprises positioning the closure in the opening such that at least a portion of the closure periphery is proximate the material memory portion. [21" id="US-20010000373-A1-CLM-00021] 21. The method of claim 20 wherein the material memory portion is an annular flange defining the opening, and wherein the step of positioning comprises positioning the closure insert across the container opening such that the closure rim is proximate the annular flange. [22" id="US-20010000373-A1-CLM-00022] 22. The method of claim 19 wherein the annular flange furthercomprises a flange extension, and wherein the method further comprises the step of shaping the flange extension to conform to the shape of the closure insert during or subsequent the step of heating. [23" id="US-20010000373-A1-CLM-00023] 23. The method of claim 18 wherein the closure periphery further comprises an outwardly facing groove and wherein the method further comprises the step of pressing a portion of the material memory portion substantially into the closure periphery groove during or subsequent the step of heating, whereby an enhanced seal between the closure periphery and container is realized. [24" id="US-20010000373-A1-CLM-00024] 24. A method of manufacturing a container having a closure, the method comprising the steps of: blow molding a container comprising a body and an accommodation element from a thermoplastic material, the accommodation element comprising an annular flange having a horizontal, radially extending portion and a vertical, axially oriented portion extending upwards from an edge thereof, the horizontal and vertical portions defining an inwardly facing, circumferential corner, and the material of the body and at least a portion of the accommodation element proximate the body being biaxially oriented via the blow molding process; trimming and removing a portion of the accommodation element above the vertical portion of the annular flange in order to provide a container opening defined by the annular flange; providing a closure insert having a closure periphery; positioning the closure insert across the container opening such that at least a portion of the closure periphery rests in the corner of the annular flange; and heating the annular flange sufficient to shrink the annular flange to engage and conform to the portion of the closure periphery resting in the corner of the annular flange. [25" id="US-20010000373-A1-CLM-00025] 25. A method of closing a container comprising the steps of: providing a container having at least one generally planar portion, the container defining an opening, and the container having at least one flap integral with the at least one generally planar portion, the at least one flap extending beyond the opening, and the container having at least one portion having a longitudinal material memory, the at least one material memory portion being proximate a junction between the at least one flap and the at least one generally planar portion; and heating the material memory portion sufficient to cause the material memory portion to longitudinally contract, the at least one flap thereby generally folding over to at least partially cover the opening.
类似技术:
公开号 | 公开日 | 专利标题 US6564531B2|2003-05-20|Blow molded container with memory shrink closure attachment and method of making the same US6062408A|2000-05-16|Wide mouth hot fill container US6237791B1|2001-05-29|Wide mouth hot fill container US4345692A|1982-08-24|Closure cap for a container CA1317556C|1993-05-11|Hot fill container EP0277557B1|1992-09-16|Blow molded plastic container US4649068A|1987-03-10|Preform for use in blow molding a container subjected to hot filling and closed by a rotatable closure, and method of an apparatus for making the same US8047390B2|2011-11-01|Container having vacuum panels US4187276A|1980-02-05|Method of making a plastic package US4927680A|1990-05-22|Preform and method of forming container therefrom US4796766A|1989-01-10|Plastic container and method of forming same US4219124A|1980-08-26|Plastic package US7918355B2|2011-04-05|Blow-molded container having thread groove CA1217911A|1987-02-17|Method for manufacturing synthetic resin can bodies US20050003123A1|2005-01-06|Preform assembly, container assembly and method of manufacture JP2007533488A|2007-11-22|Tamper-evident type closure AU2002222028B2|2006-08-31|Method for making heat-shrinkable skirt caps and resulting caps US5874141A|1999-02-23|Injection/blow molded plastic container and method EP0091275A2|1983-10-12|Improved plastic container and method of forming same JPH11152122A|1999-06-08|Biaxially stretched blow-molded bottle and its manufacture EP3375593B1|2019-06-12|Method for forming a container with a plastic liner and fibre-based shell by blow molding, preform and container US5756172A|1998-05-26|Antinesting preforms for blow molded containers AU684390B2|1997-12-11|A stretch blow moulded threaded container CA1332155C|1994-09-27|Hot fill container
同族专利:
公开号 | 公开日 US6564531B2|2003-05-20|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题 US20020117163A1|1999-10-15|2002-08-29|Thermotic Developments Limited|Self-heating of self-cooling containers| US20040159983A1|2002-08-20|2004-08-19|Sonoco Development, Inc.|Method and apparatus for blow-molding an article having a solid radially outwardly projecting flange| EP1716052A1|2003-10-15|2006-11-02|Valko Liubenov Stoilov|Method for manufacturing plastic packages and can type packages manufactured according to this method| US20070045218A1|2005-08-26|2007-03-01|Universal Solutions, Llc|Beverage container and method for making same| WO2008098602A1|2007-02-15|2008-08-21|Bernd Hansen|Receptacle| US20100301512A1|2009-05-26|2010-12-02|Gm Global Technology Operations, Inc.|Packaging and de-packaging methods using shape memory polymers| US20120193371A1|2009-08-12|2012-08-02|Akzo Nobel Swire Paints Limited|Process for producing canned product and canned product| US20160321885A1|2014-05-14|2016-11-03|Unlimited Liability, LLC|Smart memory material lock devices| WO2019013896A1|2017-07-12|2019-01-17|Dirtt Environmental Solutions, Inc.|Wall seal|US174821A||1876-03-14||Improvement in cans | US117236A||1871-07-18||Improvement in caps for preserve-jars | US29651A||1860-08-14||leland | FR575292A|1924-01-07|1924-07-26|App Magondeaux Soc D|Manufacturing process for steel tank bottoms intended to withstand high pressures| CH119342A|1926-03-23|1927-03-01|Mauser Alfons Ing Dr|Packaging container.| US2214399A|1938-11-07|1940-09-10|Continental Can Co|Closure for containers| US2532227A|1945-04-18|1950-11-28|Smith Corp A O|Pressure container for water softeners and the like| US3086679A|1960-10-11|1963-04-23|Inland Steel Container Company|Shipping container| US3296345A|1963-10-29|1967-01-03|Fmc Corp|Method of making molded containers| US3307602A|1964-05-13|1967-03-07|Samuel B Boster|Thin walled container and closure therefor| US3409710A|1965-01-19|1968-11-05|Continental Can Co|Method of molding dual wall container and closure| US3504817A|1968-05-14|1970-04-07|Owens Illinois Inc|Closure and method of applying same| US3694540A|1970-03-02|1972-09-26|Dominion Luggage Co Ltd|Method for applying bumper strip to luggage piece| US4040233A|1970-09-14|1977-08-09|Valyi Emery I|Method of obtaining a filled, fluid barrier resistant plastic container| US3791098A|1971-02-08|1974-02-12|Gillette Co|Method of manufacturing a pressurized dispensing package| DE2236528A1|1972-07-21|1974-01-31|Dichter Hans Joachim|GLASS CONTAINER WITH STOPPER| US3888347A|1973-08-06|1975-06-10|Thomas Rollin Kramer|Inflated containers for fluid pressurized balls| FR2274343B1|1974-06-11|1976-10-15|Charbonnages De France|| CA1040585A|1974-08-19|1978-10-17|Albert Obrist And Co.|Closure for containers| DE2446206A1|1974-09-27|1976-04-08|Holstein & Kappert Maschf|METHOD AND DEVICE FOR THE REMOVAL OF DISCONTINUING FUEL REMAINS| DE2606355C2|1975-02-20|1983-07-14|Carnaud Total Interplastic, Chalon-sur-Saone|Process for producing a biaxially oriented hollow body| US4000839A|1975-05-21|1977-01-04|Charles Tecco|Safety closure with removable lid for containers| NL185713C|1975-09-12|1990-07-02|Akerlund & Rausing Ab|METHOD FOR MANUFACTURING GAS-PROOF PLASTIC HOLDER| US4265852A|1977-08-01|1981-05-05|National Can Coporation|Process for forming a plastic article| US4264010A|1978-10-04|1981-04-28|Mitsubishi Plastics Industries, Ltd.|Heat shrinkable polyvinyl chloride film| US4226334A|1978-12-14|1980-10-07|Automatic Liquid Packaging, Inc.|Stopper| CH646398A5|1980-03-28|1984-11-30|Obrist Ag Albert|METHOD AND DEVICE FOR SCREWING ON A CAP FROM PLASTIC MATERIAL ON A CONTAINER MOUNT.| DE3033821C2|1980-09-09|1982-09-09|Gerhard 7166 Sulzbach-Laufen Hansen|Method and device for producing a container from a heat-sealable plastic tube and containers produced by the method and by means of the device| JPH0156892B2|1981-05-19|1989-12-01|Yoshino Kogyosho Co Ltd|| US4576843A|1981-11-23|1986-03-18|The Continental Group, Inc.|Blow molded containers and method of forming the same| US4566923A|1983-05-27|1986-01-28|Osgood Industries, Inc.|Method and apparatus for preforming and applying a heat-shrinkable member to a container| US5248533A|1984-02-15|1993-09-28|Yoshino Kogyosho Co., Ltd.|Biaxially oriented polyethylene terephthalate resin bottle-shaped container| US4578028A|1984-12-06|1986-03-25|The Procter & Gamble Company|Expandable core pin for blow-molding a container having a neck-portion with internal attachment means| US4642254A|1985-03-19|1987-02-10|Monsanto Company|Process and device for temporarily holding and releasing objects| US4607757A|1985-04-02|1986-08-26|Continental White Cap, Inc.|Anti-spin interference fit of press-seal insert and method of assembly| DE3668867D1|1986-01-27|1990-03-15|Scheidegger W & Cie Sa|METHOD AND DEVICE FOR PRODUCING A SCREW CAP FOR CONTAINERS WITH A NECK WITH EXTERNAL THREAD.| US4813807A|1985-09-24|1989-03-21|Grumman Aerospace Corporation|Memory metal connector for panels| FR2613707B1|1987-04-07|1991-05-03|Fuso Pharmaceutical Ind|METHOD AND DEVICE FOR SEALING THE NUT OF A SYNTHETIC RESIN TRANSFUSION CONTAINER| US4787531A|1988-02-22|1988-11-29|Emerson Electric Co.|Cover and seal for power driven threading machine oil reservoir| US5054272A|1990-08-06|1991-10-08|Graham Engineering Corporation|Method for sealing blow molded bottle| US5200587A|1990-10-22|1993-04-06|Fmc Corporation|Induction heating coil with conical base| FR2669989B1|1990-12-03|1993-04-02|Plastic Omnium Cie|PIPING ELEMENT PROVIDED WITH A FLANGE, ITS MANUFACTURING METHOD AND JUNCTION OF SUCH A FLANGE ELEMENTS.| US5234130A|1991-03-22|1993-08-10|Manhattan Products, Inc.|Dispensing package for a pourable material having a bottle, a pour-back spout and a closure| US5275767A|1991-06-19|1994-01-04|Micciche Frank S|Manufacture of plastic containers| US5120175A|1991-07-15|1992-06-09|Arbegast William J|Shape memory alloy fastener| US5378421A|1993-03-22|1995-01-03|Pepsico, Inc.|Process for preparing thermoplastic containers| US5351462A|1993-06-02|1994-10-04|Automatic Liquid Packaging, Inc.|Method and apparatus for installing an insert to seal a container| DE69414765T2|1993-06-30|1999-05-06|Hitachi Ltd|Shape memory pipe coupling for underwater pipes| US5484244A|1994-02-07|1996-01-16|Mse, Inc.|Self-locking threaded fasteners| JP3047732B2|1994-05-16|2000-06-05|東洋製罐株式会社|Manufacturing method of biaxially stretched blow container| US5661889A|1995-01-12|1997-09-02|Valyi; Emery I.|Process for producing a container and closure assembly| US5836066A|1996-07-22|1998-11-17|Innovative Dynamics, Inc.|Process for the production of two-way shape memory alloys|US6962338B2|2002-02-22|2005-11-08|Jds Uniphase Inc.|Hermetic seal and a method of making such a hermetic seal| GB2417875B|2004-09-01|2009-01-28|Quickwave Internat Corp|Cooking apparatus and method of use| MX2008016021A|2006-06-14|2009-01-15|Glad Products Co|Trash receptacle with dispensable bags.| DE102006061120B4|2006-12-22|2011-12-22|Khs Gmbh|Keg| US20090100805A1|2007-10-19|2009-04-23|Schneider Wayne F|Sealed plastic closure and method for making the same| AT508042A2|2009-03-24|2010-10-15|Alutech Gmbh|WORKSHOP UNIT WITH A TEMPERATURE-SENSITIVE VEHICLE COMPOUND| US9850064B2|2011-06-27|2017-12-26|Charles Christopher Egan|Waste receptacle having sealed replacement liner storage|
法律状态:
2006-11-20| FPAY| Fee payment|Year of fee payment: 4 | 2010-11-22| FPAY| Fee payment|Year of fee payment: 8 | 2014-12-24| REMI| Maintenance fee reminder mailed| 2015-05-20| LAPS| Lapse for failure to pay maintenance fees| 2015-06-15| STCH| Information on status: patent discontinuation|Free format text: PATENT EXPIRED DUE TO NONPAYMENT OF MAINTENANCE FEES UNDER 37 CFR 1.362 | 2015-07-07| FP| Expired due to failure to pay maintenance fee|Effective date: 20150520 |
优先权:
[返回顶部]
申请号 | 申请日 | 专利标题 US28785099A| true| 1999-04-07|1999-04-07|| US09/739,177|US6564531B2|1999-04-07|2000-12-18|Blow molded container with memory shrink closure attachment and method of making the same|US09/739,177| US6564531B2|1999-04-07|2000-12-18|Blow molded container with memory shrink closure attachment and method of making the same| 相关专利
Sulfonates, polymers, resist compositions and patterning process
Washing machine
Washing machine
Device for fixture finishing and tension adjusting of membrane
Structure for Equipping Band in a Plane Cathode Ray Tube
Process for preparation of 7 alpha-carboxyl 9, 11-epoxy steroids and intermediates useful therein an
国家/地区
|