专利摘要:
An improved arc-welding process and apparatus for producing welded seams by means of band or flat strip electrodes. The apparatus of the invention uses at least two band or flat strip electrodes which overlap at least partially. The aformentioned flat strip electrodes are then welded by means of arc-welding in a common welding bath.
公开号:SU741785A3
申请号:SU701604403
申请日:1970-12-24
公开日:1980-06-15
发明作者:Шерл Петер
申请人:Ферайнигте Едельштальверке Акциенгезельшафт (Феб) (Фирма);
IPC主号:
专利说明:

one
The invention relates to the welding industry and can be used in the surfacing of wide surfaces in the manufacture of new and repair of worn parts in machinostroy- 5
SRI.
The known method of arc wide-layer surfacing, in which the electrode feed is performed in such a way that the axis of the weld bead is located perpendicular to the plane of the tape. In this case, the width of the weld bead is almost equal to the width of the tape electrode 1.
The disadvantage of this method is that it is necessary to vary the width of the ribbon electrode, depending on the need to obtain a certain width of the weld bead.
The closest to the described 20 invention to the technical essence and the achieved result is a method of arc welding with simultaneous supply of at least two tape electrodes to the total welding bath 25 2.
The disadvantage of this method is that the electrodes are supplied congruently, which leads to an increase in Dimensional sizes; 1 electrode tape for 30
2
I get a certain width of the weld bead.
The aim of the invention is to improve the reflow performance with minimal penetration.
This goal is achieved by the fact that tape-type electrodes are positioned (perpendicular to the direction of welding with a degree of overlap within 16100% of the width of the electrodes. In addition, at a 100% degree of overlap, the tape-type electrodes are positioned with a gap of 2-10 mm between the wide sides in welding.
FIG. 1, 2 and 3 shows the arrangement of tape electrodes with different magnitude of overlap.
Electrodes of any shape, the width of which is much greater than their thickness, can be used as tape electrodes. The ratio of the width to the thickness of the tape electrodes lies in the range between 360: 1 and 3: 1. The most commonly used tape electrodes are 60 X 0.5 mm in size, which corresponds to a ratio of width to thickness of 120: 1.
It is possible to perform welding with strip electrodes of different composition.
Example 1. Conducted surfacing two tape electrodes of austenitic class under the flux on the undoped structural steel (C 0.08%, Si 0.026%, Mp 0.45%). The size of the electrodes is 60 X 0.5 mm, the overlap is 10 mm, the welding speed is 15 cm / min, the welding current is 990 A, the voltage is 30 V.
A satisfactory deposition was obtained (bead width 110 mm, height 4.6 mm). Roller smooth and smooth. In the eon overlap, the rise is not formed.
Example 2.-The deposition was carried out using three ribbon electrodes of 60 x 0.5 mm in size, whose composition is the same as in example 1. Welding mode: DCB 1250-1350 A, Ucg 30 V, speed 13 cm / min. Electrode Offsets Shown in FIG. one.
权利要求:
Claims (2)
[1]
1. The method of arc welding with simultaneous filing of at least two
two tape electrodes into a common weld pool, characterized in that, in order to increase the reflow performance with minimum penetration, the tape electrodes are arranged perpendicular to the welding direction with a degree of overlap within 16-100% of the electrode width.
[2]
2. The method according to claim 1, is also distinguished by the fact that at a 100% degree of overlapping, the tape electrodes are positioned with a gap of 2-10 mm between the wide sides in the welding direction.
Sources of information taken into account in the examination
1.Ignatov V.A. and others. Automatic machine for welding and welding with a tape electrode, Welding production, -1974, No. 1, p. 29, 50.
2. USSR author's certificate
 197822, cl. At 23 K 9/04, 28.04.66.
SSaWy S
fat. g
g.Z.
类似技术:
公开号 | 公开日 | 专利标题
SU741785A3|1980-06-15|Method of arc fusing on
SE7607639L|1977-04-06|DEVICE FOR PLATING A WORK PIECE WITH AN ELECTRO BRAKE
US3704358A|1972-11-28|Submerged-arc both-side butt welding method of a square groove
US3549856A|1970-12-22|Gas metal arc welding from one side
US3171944A|1965-03-02|Method of submerged arc welding of fillet welds
US3832523A|1974-08-27|Method for electrical arc welding
US3748429A|1973-07-24|Multiple-wire single-pass submerged-arc welding method for thick plates
GB1052407A|
GB990208A|1965-04-28|Improvements in or relating to welding processes
US3617690A|1971-11-02|Automatic narrow-gap joint welding method with multiple electrodes
US1267400A|1918-05-28|Method of treating electrodes for electric welding.
SU1237347A1|1986-06-15|Method of multielectrode arc working of metals
SU941052A1|1982-07-07|Method of automatic arc welding
SU1109273A2|1984-08-23|Process for two-electrode arc welding
SU544526A1|1977-01-30|Arc welding method
SU78667A1|1948-11-30|Argon arc welding method
SU692712A1|1979-10-25|Method of fusion welding of different metals
US3710066A|1973-01-09|Method of electric-arc welding of tubular products with magnetic control of the arc
SU707710A1|1980-01-05|Method of electric-arc multipass welding
SU592539A1|1978-02-15|Method of electric arc welding with consumable electrode
SU1590269A2|1990-09-07|Method of one-sided arc welding of two-layer steels
SU397288A1|1973-09-17|In PTB
SU1555077A1|1990-04-07|Method of wide-layer surfacing
US3601579A|1971-08-24|Method of welding metal parts and articles
SU595102A1|1978-02-28|Electric arc cutting method
同族专利:
公开号 | 公开日
NO132750C|1976-01-07|
NL156626B|1978-05-16|
CA932405A|1973-08-21|
TR17539A|1975-07-23|
DE2000037C3|1979-07-12|
ZA708649B|1971-09-29|
NL7018799A|1971-06-28|
NO132750B|1975-09-22|
DE2000037A1|1971-07-01|
AT313026B|1974-01-25|
FR2074129A5|1971-10-01|
BE760859A|1971-05-27|
GB1332915A|1973-10-10|
CH536158A|1973-04-30|
DE2000037B2|1975-10-23|
ES386697A1|1974-06-16|
US3751628A|1973-08-07|
SE374290B|1975-03-03|
HU162738B|1973-04-28|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题
WO2017127039A1|2016-01-18|2017-07-27|Андрей Иванович ПАНФИЛОВ|Method for overlay welding a wear resistant coating|US2083309A|1935-01-09|1937-06-08|Robert R Applegate|Method and apparatus for welding|
US2091871A|1935-11-11|1937-08-31|Braunschweiger Huttenwerk G M|Method of welding alloys to a base metal|
US2151914A|1936-09-16|1939-03-28|Kellogg M W Co|Welding apparatus|
AT239038B|1961-11-25|1965-03-10|Boehler & Co Ag Geb|Method and device for welding, in which two partially sheathed electrodes are brought together after the power supply at the welding point to form an electrode sheathed on all sides|
US3271554A|1965-06-24|1966-09-06|Arcos Corp|Overlay welding|
US3358115A|1966-11-28|1967-12-12|Roman F Arnoldy|Open arc or gas shielded granular welding|US3832523A|1972-04-17|1974-08-27|Osaka Transformer Co Ltd|Method for electrical arc welding|
US4000373A|1975-02-24|1976-12-28|Allegheny Ludlum Industries, Inc.|Strip electrode for overlay welding|
US4303821A|1979-11-19|1981-12-01|David J. Eastin|Strip welding for butt joints|
SE439608B|1980-02-19|1985-06-24|Esab Ab|WELD HEAD WITH A FEEDING WORK FOR PROMOTING ATMINSTONE A BANDLE ELECTRODE|
US4593174A|1982-04-23|1986-06-03|Nippon Steel Corporation|Method for welding very low carbon steel|
US5155330A|1991-08-02|1992-10-13|The Lincoln Electric Company|Method and apparatus for GMAW welding|
DE19953079B4|1999-11-04|2013-12-19|Alstom Technology Ltd.|Method for welding components|
SE530969C2|2007-03-06|2008-11-04|Esab Ab|Connectors and welding apparatus|
US20090188896A1|2008-01-25|2009-07-30|Gm Global Technology Operations, Inc|GMAW System Having Multiple Independent Wire Feeds|
US8952292B2|2012-04-17|2015-02-10|Caterpillar Inc.|Adjustable welding head for multiple electrode cladding|
EP2938453B1|2012-12-28|2018-02-14|Esab AB|Arc welding method and arc welding arrangement with first and second electrodes|
ITUA20162979A1|2016-04-28|2017-10-28|Illinois Tool Works|HEADS FOR RIBBON PLATING WITH RIBBON PRESSURE LIMITS AND RIBBON BANDING SYSTEMS WITH HEADS FOR RIBBON BANDING WITH RIBBON PRESSURE LIMITS|
ITUA20162975A1|2016-04-28|2017-10-28|Illinois Tool Works|TAPE FEEDERS FOR PLATING HAVING INDEPENDENT PRESSURE ROLLERS AND TAPE PLATING SYSTEMS WITH TAPE FEEDERS FOR PLATING HAVING INDEPENDENT PRESSURE ROLLERS|
ITUA20162983A1|2016-04-28|2017-10-28|Illinois Tool Works|HEADS FOR RIBBON PLATING HAVING INDEPENDENT BELT PRESSURE ADJUSTMENTS AND RIBBON BANDING SYSTEMS WITH HEADS FOR RIBBON BANDING WITH INDEPENDENT BELT PRESSURE ADJUSTMENT|
ITUA20162977A1|2016-04-28|2017-10-28|Illinois Tool Works|TAPE FEEDERS FOR PLATING HAVING ADJUSTABLE RIBBON GUIDES AND RIBBON PLATING SYSTEMS WITH TAPE FEEDERS FOR PLATING HAVING ADJUSTABLE RIBBON GUIDES FOR THE RIBBON|
ITUA20162981A1|2016-04-28|2017-10-28|Illinois Tool Works|RELEASE DEVICES FOR A GRANULAR WELDING FLOW AND TAPE PLATING SYSTEMS WITH RELEASE DEVICES FOR A GRANULAR FLOW|
CN107262865B|2017-05-19|2019-05-17|四川大学|A kind of hand-held tin soldering equipment|
CN111074138A|2019-12-31|2020-04-28|江苏新华合金有限公司|3944 solder strip and production process thereof|
法律状态:
优先权:
申请号 | 申请日 | 专利标题
AT1204769A|AT313026B|1969-12-24|1969-12-24|Arc fusion welding process|
[返回顶部]